ECSAINE GS for Industrial Applications:
Major Properties
| |
|
ECSAINE(Dyed) |
|
|
GS FELT |
|
|
|
|
|
Testing Method |
| |
|
|
|
|
|
|
|
|
|
(EE310SS) |
|
| ASTM D3886 P800 |
|
3000J |
700W |
100E |
500R |
K40008S |
12106NM |
K10021M |
K10250D |
K10010D |
12109NM |
|
| Composition |
Polyester(%) |
65 |
65 |
65 |
65 |
65 |
75 |
65 |
60 |
65 |
80 |
|
| |
Polyurethane(%) |
35 |
35 |
35 |
35 |
35 |
25 |
35 |
40 |
35 |
20 |
|
| Denier |
|
0.14 |
0.14 |
0.14 |
0.14 |
0.14 |
0.04 |
0.14 |
0.14 |
0.14 |
0.04 |
|
| Effective Width(mm) |
|
1360 |
1150 |
1150 |
1200 |
1150 |
1150 |
1150 |
1200 |
1150 |
1150 |
|
| Thikness(mm) |
|
0.49 |
0.55 |
0.8 |
1.2 |
0.8 |
0.6 |
2.1 |
3 |
1 |
0.9 |
Dial Thickness Gauge |
| Weight(g/㎡) |
|
115 |
125 |
220 |
355 |
225 |
230 |
565 |
910 |
280 |
350 |
|
| Tensil Strength(kg/cm) |
Longitudinal |
3 |
3.1 |
7.2 |
- |
7.3 |
11.1 |
24.9 |
33.2 |
11.3 |
16.8 |
ASTM D5035 |
| |
Transverse |
2.5 |
2 |
6.2 |
- |
5.8 |
8.2 |
22.9 |
35.8 |
10.3 |
15.3 |
|
| Tensil Elongation(%) |
Longitudinal |
56.2 |
63.9 |
83.1 |
- |
79 |
78.4 |
109.6 |
115.7 |
85.5 |
86.8 |
|
| |
Transverse |
77.8 |
112.3 |
122.7 |
- |
128.3 |
132 |
171.7 |
164.8 |
145.6 |
130.1 |
|
| Tear Strength(kg) |
Longitudinal |
0.46 |
0.9 |
1.1 |
- |
2.4 |
2.7 |
6.9 |
6.5 |
3 |
3.5 |
ASTM D1424 |
| |
Transverse |
0.31 |
0.4 |
0.9 |
- |
1.1 |
1.4 |
4.7 |
5.7 |
2.7 |
2.4 |
|
| Surface Abrasion Resistance(Times) |
|
321 |
117 |
1057 |
- |
1668 |
1637 |
>10000 |
>10000 |
3528 |
4747 |
|
|